Fixing stringing and adhesion
Many problems with PCTG and other copolyesters come down to temperature, moisture, or the build surface. Work through these checks in order.
Stringing and wisps
- Check for moisture. Popping or hissing sounds and a rough surface can mean the filament has picked up moisture. Drying it following the maker's guidance often reduces stringing.
- Lower the nozzle temperature slightly, staying within your filament maker's recommended range. A temperature tower helps find the sweet spot.
- Tune retraction in small steps. Too little can leave strings; too much can cause clogs or gaps. Stay within what your extruder maker recommends.
- Increase travel speed and enable your slicer's options to avoid crossing perimeters where available.
- Check wipe and coasting settings in your slicer, changing one setting at a time.
Blobs and buildup on the nozzle
- Raise the first layer height slightly so the nozzle is not dragging through plastic.
- Clean the nozzle while it is hot, following your printer maker's instructions.
- A nozzle with a non-stick coating or a silicone sock may help reduce buildup.
Prints not sticking
- Clean the bed according to the bed maker's instructions to remove oils and dust.
- Re-level or adjust Z offset. The first layer should be lightly pressed down, not round and loose.
- Raise the bed temperature slightly while staying within the limits recommended by your printer and filament manufacturer.
- Slow the first layer and reduce first-layer fan speed.
- Add a brim for small or tall parts.
Prints sticking too well
- Use a release layer such as glue stick on smooth surfaces, or switch to textured PEI.
- Let the bed cool fully before removing the part.
- Avoid over-squishing the first layer.
Warping on large parts
PCTG usually warps less than materials like ABS, but large flat parts can still lift. A brim, a clean bed, and keeping the printer out of drafts often help.
Back to the PCTG printing guide.